Need Help?

How should the pigments be dosed?


From 2% to 30% by weight.

It depends above all on the ability of the resin, varnish or plastic to take the load without cracking. Also, the thicker the layer, the less pigment is needed.

FAQs From Same Category

How long does phosphorescence last?

It depends on several factors:

  • First of all the colour (green and turquoise glow the longest),
  • The duration, type and intensity of the light exposure,
  • The type of material or paint (and its pigment concentration or number of coats).

How can phosphorescent products be charged most effectively?

Our photoluminescent signage guide gives a detailed list of more and less effective lighting. White and blue light are the most effective. All our products charge perfectly even in surroundings lit at only 25 lux.


Which resins should I choose?

For thin layers up to 1 cm: our 4000 resin.

For layers thicker than 1 cm: our WWA resin.